KISUMA?5P-C Magnesium Hydroxide
[Low smoke halogen-free flame retardant]
Surface treated by silane coupling agent. With excellent tensile strength property.
Typical Analysis Data |
Items | Typical Value |
Mg(OH)2% | 99.95 |
Loss on Drying(120℃ X 1Hr)% | 0.07 |
Specific Surface Area(BET)m2/g | 5.4 |
Particle Size (D50) μm | 0.95 |
≥5μm % | 0 |
KISUMA?5P-C Magnesium Hydroxide
[Low smoke halogen-free flame retardant]
Surface treated by silane coupling agent. With excellent tensile strength property.
Typical Analysis Data |
Items | Typical Value |
Mg(OH)2% | 99.95 |
Loss on Drying(120℃ X 1Hr)% | 0.07 |
Specific Surface Area(BET)m2/g | 5.4 |
Particle Size (D50) μm | 0.95 |
≥5μm % | 0 |